Effects of impurities in lime used for iron ore sintering on its hydration characteristics
oleh: ZHANG Li, WU Sheng-li, ZHANG Yong-zhong, SU Bo, KOU Ming-yin
Format: | Article |
---|---|
Diterbitkan: | Science Press 2016-12-01 |
Deskripsi
The effects of SiO<sub>2</sub>, Al<sub>2</sub>O<sub>3</sub> and MgO on the hydration of lime were investigated by isothermal calorimetry, and the results were validated by 5 types of lime used in the sintering plant. It is found that the total hydrating heat of lime has positive relationship with CaO content, and decreases with increasing SiO<sub>2</sub>, Al<sub>2</sub>O<sub>3</sub> and MgO contents. The contents of SiO<sub>2</sub>, Al<sub>2</sub>O<sub>3</sub> and MgO also have important effect on the hydrating speed of lime. When the mass fraction of SiO<sub>2</sub> increases to 1%, the hydrating speed of lime dramatically decreases, and then slowly drops with increasing SiO<sub>2</sub> content. A small amount of Al<sub>2</sub>O<sub>3</sub> has no significant effect on the hydrating speed of lime, but when the mass fraction of Al<sub>2</sub>O<sub>3</sub> is more than 2%, the hydrating speed of lime sharply decreases. With the increase of MgO content, the hydrating speed of lime significantly decreases.