Aggregate Suitability of the Late Permian WargalLimestone at Kafar Kot Chashma Area, Khisor Range, Pakistan

oleh: Rizwan Ullah, Shuja Ullah, Nazir Rehman, Fayyaz Ali, Muhammad Asim, Muhammad Tahir, Subhan Ullah, Shafi Muhammad

Format: Article
Diterbitkan: Society of Economic Geologists and Mineral Technologists 2020-07-01

Deskripsi

This study was carried out for the investigationofthe Late Permian Wargal limestone at Kafar Kot Chashmaarea, Khisor Range to determine its suitability as an aggregate that is used in roadconstruction and civil structures with the help of geological engineering testing. The results of geological engineering testing of Wargal limestone samples show the tolerable values of all standard engineering parameters including the Loss Angles Abrasion value (23.37%), Aggregate impact (16.8%), Crushing value 13.1%, Unit weight 1.67, Soundness (1.007%), Specific gravity (2.70), Water Absorption (0.48%), Flakiness Index (6.5%), Elongation value(7.1%), Coating of bitumen (> 95%), stripping of bitumen (<5%), California Bearing Ratio(CBR) value (93.6%), Maximum Dry Density 2.307g/c and Optimum Moisture Content (5.79%). As per different International and National Standards like AASHTO, ASTM, BS and NHA, the mentioned results of various engineering tests were within the tolerable limits. The petrography of the selected samples of the Late Permian Wargal limestone revealed very minor value of quartz (0.5%), hematite/limonite (0.6%) and clay content 1.0% showing the insignificant threat of ASR. The values of dolomite are limited to (1%) which shows that there is no ACR reaction with ordinary Portland cement. The results of geological and engineering parameters of the study areastrongly suggest its suitability as a potential aggregate (i.e. for the base course, subbase course, cement concrete and asphalt) in the road construction.